Grade 7 (CP + Pd (Enhanced Corrosion Resistance)) — Properties, Specifications & Supply
Density
4.51 g/cm3
Melting Point
1665 °C
Tensile Strength
345–450 MPa
Yield Strength
275–410 MPa
Elastic Modulus
103 GPa
UNS Number
R52400
Chemical Composition
| Ti | Pd | Fe | O | C | N | H |
|---|---|---|---|---|---|---|
| Balance | 0.12-0.25 | ≤ 0.3 | ≤ 0.25 | ≤ 0.08 | ≤ 0.03 | ≤ 0.015 |
Values in wt%. Single values indicate maximum allowable content.
Mechanical Properties
| Property | Value | Unit |
|---|---|---|
| Ultimate Tensile Strength | 345 – 450 | MPa |
| Yield Strength (0.2% Offset) | 275 – 410 | MPa |
| Elongation at Break | ≥ 20 | % |
| Hardness | 200 | HB |
| Elastic Modulus | 103 | GPa |
| Density | 4.51 | g/cm³ |
| Melting Point | 1665 | °C |
International Grade Equivalents
| Standard | Designation |
|---|---|
| ASTM (USA) | Grade 7 |
| GB/T (China) | TA9 |
| DIN/EN (Germany/EU) | 3.7235 |
| GOST (Russia) | — |
| JIS (Japan) | — |
| UNS (Unified) | R52400 |
Applicable Specifications
Weight Calculator for Grade 7
Berechnetes Gewicht
Kostenschätzung (FOB Baoji)
* Nur Richtpreise. Das tatsächliche Angebot hängt von Spezifikationen, Toleranzen und Zertifizierungsanforderungen ab.
Grade 5 Eigenschaften
Request a Quote for Grade 7
We supply Grade 7 (CP + Pd (Enhanced Corrosion Resistance)) in sheets, plates, bars, tubes, forgings, and custom forms. Certified to ASTM B265 and other applicable standards.
Get a Quote →Other Titanium Grades
Grade 1
Commercially Pure
240–345 MPa
Grade 2
Commercially Pure
345–450 MPa
Grade 4
Commercially Pure (High Strength)
550–680 MPa
Grade 5
α+β Alloy (Ti-6Al-4V)
895–1000 MPa
Grade 9
Near-α Alloy (Ti-3Al-2.5V)
620–750 MPa
Grade 12
Near-α (Ti-0.3Mo-0.8Ni)
483–620 MPa
Grade 23
α+β ELI (Ti-6Al-4V ELI)
828–965 MPa