ASTM B861 Standard Specification for Titanium and Titanium Alloy Seamless Pipe

Scope

Covers titanium and titanium alloy seamless pipe for general corrosion resisting and elevated temperature service.

Covered Product Forms

Seamless Pipe

Key Requirements

  • Chemical composition
  • Mechanical properties
  • Hydrostatic test
  • UT inspection

Test Methods

  • ASTM E8
  • ASTM E213
  • ASTM E1409

Related Specifications