Elija IrO₂–Ta₂O₅ (70:30) para evolución de oxígeno (OER) en baños ácidos de sulfato/nitrato y electrodeposición de metales; elija RuO₂–IrO₂ para evolución de cloro (CER) en plantas cloro-álcali, agua de mar e hipoclorito.

Propiedad IrO₂–Ta₂O₅ Coating (OER) RuO₂–IrO₂ Coating (CER)
Reacción electroquímica principal Oxygen Evolution (OER) Chlorine Evolution (CER)
Estabilidad en sulfatos/nitratos ácidos Exceptional (H₂SO₄, HNO₃) ★ Poor — RuO₂ dissolves rapidly in OER
Sobrepotencial de cloro (energía) Higher (less efficient for Cl₂) Very Low (maximum energy savings) ★
Typical OER Lifespan (Acidic) (Years) 3–8+ years (multi-year continuous) ★ <1 year if forced into acidic OER
Typical CER Lifespan (Brine) (Years) Moderada 5–10+ years (chlor-alkali / NaClO) ★
Recommended Substrate ASTM B265 Grade 1 or Grade 2 Ti ASTM B265 Grade 1 or Grade 2 Ti
Substrate Recoatability Strippable & recoatable Strippable & recoatable
Key Industrial Applications Cu/Zn electrowinning, copper foil, PEM, ICCP, wastewater Chlor-alkali, hypochlorite, seawater, pool chlorinators

Elija IrO₂–Ta₂O₅ Coating (OER) cuando

  • ✓ Copper foil production, Cu/Zn/Ni electrowinning, and acidic sulfate baths
  • ✓ Industrial wastewater COD oxidation and high-potential OER cells
  • ✓ Impressed Current Cathodic Protection (ICCP) in soil or fresh water
  • ✓ Low-chloride or chloride-free electrolytes where O₂ is the main gas

Elija RuO₂–IrO₂ Coating (CER) cuando

  • ✓ Chlor-alkali membrane cells and brine electrolysis
  • ✓ On-site sodium hypochlorite (NaClO) and ballast water chlorination
  • ✓ Seawater electrochlorination and swimming pool salt cells
  • ✓ High-chloride neutral brines prioritizing minimum kWh per kg of Cl₂

Preguntas técnicas frecuentes

What happens if a RuO2-IrO2 anode is used in a sulfuric acid copper electrowinning bath?
In chloride-free sulfuric acid, oxygen evolution is the sole anode reaction. RuO2 oxidizes to volatile/soluble RuO4 at oxygen-evolution potentials, causing rapid coating loss and voltage spikes. IrO2-Ta2O5 is mandatory for sulfuric acid OER service.
Can spent IrO2-Ta2O5 or RuO2-IrO2 titanium anodes be stripped and recoated?
Yes. As long as the Grade 1 or Grade 2 titanium base mesh or plate has not suffered fluoride corrosion or severe mechanical warping, the depleted oxide layer can be chemically/mechanically stripped and thermally recoated at 40–60% of the cost of fabricating new anodes.

¿No sabe qué material le conviene?

Indíquenos aplicación, entorno y presupuesto: le recomendaremos el grado óptimo.

Comparativas relacionadas

¿Listo para iniciar su proyecto?

Envíe su plano o especificación y le responderemos en un plazo de 24 horas.

Solicitar cotización
Consulta rápida
WhatsApp