Type something to search...

Nickel 200 (ASTM B161 / B163) против Titanium Grade 2 (ASTM B338)

В горячей концентрированной каустической соде (>30 % NaOH выше 80–100 °C) обязателен Никель 200 (ASTM B161/B163, <0,025 мм/год), так как титан Grade 2 подвергается гидридному охрупчиванию — при этом титан доминирует в хлорном и рассольном контурах тех же производств.

Характеристика Nickel 200 (ASTM B161 / B163) Titanium Grade 2 (ASTM B338)
UNS и стандарт труб N02200 (ASTM B161 / B163) R50400 (ASTM B338 / B861)
Горячая каустическая сода (50 % NaOH, >100 °C) Excellent (<0.025 mm/yr) ★ Poor — hydride embrittlement & corrosion
Влажный хлор / горячий рассол Poor — rapid pitting/attack Excellent (immune <80°C; Gr7 >100°C) ★
Теплопроводность (W/m·K) 70.2 ★ 21.9
Плотность (g/cm³) 8.89 4.51 ★
Tensile / Yield Strength (Annealed) (MPa) 380 / 103 (min) 345 / 275 (min) ★
Max Continuous Service Temp (°C) 315 (use Ni 201 >315°C) 315 (ASME pressure vessels)
Primary Chlor-Alkali Role Caustic evaporators & NaOH heaters Brine heaters, wet Cl₂ coolers, anodes

Выбирайте Nickel 200 (ASTM B161 / B163), если

  • ✓ 30–73% caustic soda (NaOH) or potassium hydroxide (KOH) evaporators above 80°C
  • ✓ High heat-transfer efficiency needed in alkaline falling-film evaporators
  • ✓ Synthetic fiber, food-grade caustic, and alkaline battery precursor reactors
  • ✓ ASTM B163 condenser tubes or ASTM B161 caustic transfer piping

Выбирайте Titanium Grade 2 (ASTM B338), если

  • ✓ Seawater, concentrated NaCl brine heaters, and desalination condensers
  • ✓ Wet chlorine gas coolers, hypochlorites, and oxidizing acid streams
  • ✓ Weight-sensitive heat exchangers requiring 49% lower tube bundle mass
  • ✓ Neutral or mildly alkaline media (<10% NaOH below 60°C)

Часто задаваемые технические вопросы

What is the difference between ASTM B161 and ASTM B163 for Nickel 200 tubes?
ASTM B161 covers seamless nickel pipe and general tubing specified by NPS/Schedule or OD for process piping, while ASTM B163 specifically governs seamless nickel and nickel-alloy condenser and heat-exchanger tubes with tighter dimensional tolerances, eddy-current/hydrostatic testing, and heat-transfer surface control.
Why does Titanium Grade 2 fail in hot concentrated sodium hydroxide (NaOH)?
Above roughly 80–100°C in concentrated caustic solutions (typically >30% NaOH), the protective TiO2 film slowly dissolves and atomic hydrogen generated at the surface diffuses into titanium, forming brittle titanium hydrides that cause sudden cracking.

Не уверены, какой материал подойдёт?

Сообщите применение, условия эксплуатации и бюджет — предложим оптимальную марку.

Похожие сравнения

Готовы начать свой проект?

Отправьте ваш чертёж или спецификацию, и мы ответим в течение 24 часов.

Запросить цену
Быстрый запрос
WhatsApp