Titanium Grade 7 (Ti-0.15Pd) vs. Hastelloy C-276 (UNS N10276)

El Titanio Grado 7 (4,51 g/cm³) pesa un 49 % menos que Hastelloy C-276 (8,89 g/cm³) y supera a C-276 en cloruros oxidantes calientes y cloro húmedo, mientras que Hastelloy C-276 domina en ácidos reductores concentrados y temperaturas superiores a 315 °C.

Propiedad Titanium Grade 7 (Ti-0.15Pd) Hastelloy C-276 (UNS N10276)
Designación UNS R52400 (Ti-0.15Pd) N10276 (Ni-16Mo-16Cr-4W)
Densidad (g/cm³) 4.51 (49% lighter) ★ 8.89
Cloruros oxidantes calientes / Cl₂ húmedo Superior (virtually immune) ★ Good (can pit in hot wet Cl₂ / OCl⁻)
Ácidos reductores (HCl / H₂SO₄ calientes) Moderate (dilute/moderate limits) Superior (handles severe mixed acids) ★
Resistencia a SCC por cloruros Immune Immune / highly resistant
Temp. máx. en recipientes a presión (°C) 315 (ASME Sec VIII) 675+ (high-temp superalloy) ★
Yield Strength (Min) (MPa) 275 283
Peso del material a igual volumen 0.51x baseline ★ 1.0x baseline (nearly 2x heavier)

Elija Titanium Grade 7 (Ti-0.15Pd) cuando

  • ✓ Hot oxidizing chloride brines, seawater evaporators, and wet chlorine scrubbers
  • ✓ Severe gasket or tube-to-tubesheet crevice geometries above 80°C
  • ✓ Weight-sensitive offshore skids or large-area plate heat exchangers
  • ✓ Need to lower total vessel tonnage via 49% lower metal density

Elija Hastelloy C-276 (UNS N10276) cuando

  • ✓ Process swings into concentrated, deaerated reducing HCl or H2SO4
  • ✓ Trace fluorides (HF) are present in the chemical stream
  • ✓ Operating temperature exceeds 315°C under ASME pressure rules
  • ✓ Field maintenance team lacks cleanroom/argon-purge titanium welding capability

Preguntas técnicas frecuentes

Is Titanium Grade 7 cheaper than Hastelloy C-276 for a heat exchanger?
On a per-kilogram basis their prices can be close depending on palladium and nickel spot markets, but Titanium Grade 7 has a density of 4.51 g/cm³ versus 8.89 g/cm³ for Hastelloy C-276. Because an identical tube bundle requires 49% less mass in titanium, Grade 7 frequently delivers a lower total material bill.
Which performs better in wet chlorine gas—Titanium Grade 7 or Hastelloy C-276?
Titanium Grade 7 (and even Grade 2) is the global benchmark for wet chlorine gas (>1% moisture), exhibiting near-zero corrosion. Note that titanium must NEVER be used in completely dry chlorine gas (<0.5% water), where pyrophoric ignition can occur.

¿No sabe qué material le conviene?

Indíquenos aplicación, entorno y presupuesto: le recomendaremos el grado óptimo.

Comparativas relacionadas

¿Listo para iniciar su proyecto?

Envíe su plano o especificación y le responderemos en un plazo de 24 horas.

Solicitar cotización
Consulta rápida
WhatsApp