Titanium Grade 7 (Ti-0.15Pd) vs. Titanium Grade 12 (Ti-0.3Mo-0.8Ni)

El Titanio Grado 7 (Ti-0,15Pd) protege frente a corrosión en rendijas hasta pH 1 en cloruros en ebullición, mientras que el Grado 12 (Ti-0,3Mo-0,8Ni) elimina el coste del paladio — ahorrando un 40–60 % con un 25 % más de límite elástico (345 vs. 275 MPa) en salmueras calientes de pH >= 3.

Propiedad Titanium Grade 7 (Ti-0.15Pd) Titanium Grade 12 (Ti-0.3Mo-0.8Ni)
UNS y Composición R52400 (CP Ti + 0.12–0.25% Pd) R53400 (Ti + 0.3% Mo + 0.8% Ni)
Inmunidad a corrosión en rendijas (Cl⁻) Down to pH 1 (up to >200°C) ★ pH 3–11 (up to ~200°C)
Tolerancia a ácidos reductores Best among standard Ti grades ★ Moderate (better than Gr2, below Gr7)
Resistencia a la tracción mín. (MPa) 345 483 ★
Límite elástico mín. (MPa) 275 345 ★
Elongation (Min) (%) 20 ★ 18
Weldability & Formability Excellent (identical to Gr2) ★ Very Good (ERTi-12 filler)
Relative Material Cost High (2.5–4.5× Gr2; Pd-indexed) Economical (~1.3–1.6× Gr2) ★

Elija Titanium Grade 7 (Ti-0.15Pd) cuando

  • ✓ Hot chloride brines with acidic excursions below pH 3
  • ✓ Severe crevice geometries under scale deposits or PTFE gaskets
  • ✓ Reducing acid contamination (dilute HCl / H2SO4) mixed with chlorides
  • ✓ Zero-risk replacement where failure triggers catastrophic plant shutdown

Elija Titanium Grade 12 (Ti-0.3Mo-0.8Ni) cuando

  • ✓ Hot neutral/mildly acidic brines (pH >= 3, 80–200°C) such as salt evaporators
  • ✓ ASME pressure vessels benefiting from 25% higher yield strength (345 MPa)
  • ✓ Eliminating palladium bullion price volatility from multi-ton RFQs
  • ✓ Geothermal, desalination, and refinery overhead condenser tubes

Preguntas técnicas frecuentes

How much cheaper is Titanium Grade 12 than Grade 7?
Depending on palladium market pricing and product form, Titanium Grade 12 typically costs 40% to 60% less than Grade 7 while still preventing hot-brine crevice corrosion in neutral and mildly acidic chloride solutions (pH >= 3).
What about Titanium Grade 16 as a middle option between Grade 7 and Grade 12?
Titanium Grade 16 (UNS R52402) reduces the palladium addition to 0.04–0.08% (roughly one-third of Grade 7's Pd content). It provides crevice resistance close to Grade 7 at a lower palladium surcharge, though Grade 7 and Grade 12 remain much more widely stocked in plate, bar, and ASTM B338 tubing.

¿No sabe qué material le conviene?

Indíquenos aplicación, entorno y presupuesto: le recomendaremos el grado óptimo.