Titanium Grade 7 (Ti-0.15Pd) против Titanium Grade 12 (Ti-0.3Mo-0.8Ni)

Титан Grade 7 (Ti-0,15Pd) защищает от щелевой коррозии вплоть до pH 1 в кипящих хлоридах, а Grade 12 (Ti-0,3Mo-0,8Ni) исключает дорогой палладий — снижая цену на 40–60 % при более высоком пределе текучести (345 против 275 МПа) в горячих рассолах с pH >= 3.

Характеристика Titanium Grade 7 (Ti-0.15Pd) Titanium Grade 12 (Ti-0.3Mo-0.8Ni)
UNS и состав R52400 (CP Ti + 0.12–0.25% Pd) R53400 (Ti + 0.3% Mo + 0.8% Ni)
Защита от щелевой коррозии (горячие Cl⁻) Down to pH 1 (up to >200°C) ★ pH 3–11 (up to ~200°C)
Стойкость в восстановительных кислотах Best among standard Ti grades ★ Moderate (better than Gr2, below Gr7)
Мин. предел прочности (MPa) 345 483 ★
Мин. предел текучести (MPa) 275 345 ★
Elongation (Min) (%) 20 ★ 18
Weldability & Formability Excellent (identical to Gr2) ★ Very Good (ERTi-12 filler)
Relative Material Cost High (2.5–4.5× Gr2; Pd-indexed) Economical (~1.3–1.6× Gr2) ★

Выбирайте Titanium Grade 7 (Ti-0.15Pd), если

  • ✓ Hot chloride brines with acidic excursions below pH 3
  • ✓ Severe crevice geometries under scale deposits or PTFE gaskets
  • ✓ Reducing acid contamination (dilute HCl / H2SO4) mixed with chlorides
  • ✓ Zero-risk replacement where failure triggers catastrophic plant shutdown

Выбирайте Titanium Grade 12 (Ti-0.3Mo-0.8Ni), если

  • ✓ Hot neutral/mildly acidic brines (pH >= 3, 80–200°C) such as salt evaporators
  • ✓ ASME pressure vessels benefiting from 25% higher yield strength (345 MPa)
  • ✓ Eliminating palladium bullion price volatility from multi-ton RFQs
  • ✓ Geothermal, desalination, and refinery overhead condenser tubes

Часто задаваемые технические вопросы

How much cheaper is Titanium Grade 12 than Grade 7?
Depending on palladium market pricing and product form, Titanium Grade 12 typically costs 40% to 60% less than Grade 7 while still preventing hot-brine crevice corrosion in neutral and mildly acidic chloride solutions (pH >= 3).
What about Titanium Grade 16 as a middle option between Grade 7 and Grade 12?
Titanium Grade 16 (UNS R52402) reduces the palladium addition to 0.04–0.08% (roughly one-third of Grade 7's Pd content). It provides crevice resistance close to Grade 7 at a lower palladium surcharge, though Grade 7 and Grade 12 remain much more widely stocked in plate, bar, and ASTM B338 tubing.

Не уверены, какой материал подойдёт?

Сообщите применение, условия эксплуатации и бюджет — предложим оптимальную марку.