Zirconium 702 (UNS R60702) против Zirconium 705 (UNS R60705)

По ASTM B551 цирконий 705 (Zr-2,5Nb) имеет на 85 % более высокий минимальный предел текучести, чем Zr 702 (380 против 205 МПа), позволяя уменьшить толщину стенки реакторов, но требует обязательного послесварочного отжига (~550–595 °C) для снятия напряжений.

Характеристика Zirconium 702 (UNS R60702) Zirconium 705 (UNS R60705)
UNS и состав R60702 (Zr+Hf >= 99.2%) R60705 (Zr + 2.0–3.0% Nb)
Min Tensile Strength (ASTM B551) (MPa) 380 (55 ksi) 550 (80 ksi) ★
Min Yield Strength (0.2%) (MPa) 205 (30 ksi) 380 (55 ksi) ★
Min Elongation (in 50 mm) (%) 16 16
Послесварочная термообработка (PWHT) Generally not required ★ Mandatory stress relief (~550–595°C)
Corrosion Resistance (Extreme H₂SO₄) Best (unalloyed single-phase) ★ Very Good (slightly narrower ceiling)
Bend Radius / Deep Drawing Better for complex forming ★ Good (higher springback)
Typical Equipment Application Heat exchanger tubes, vessel liners, columns High-pressure reactors, shafts, bolts, pumps

Выбирайте Zirconium 702 (UNS R60702), если

  • ✓ Heat exchanger tubes, distillation columns, and corrosion-resistant liners
  • ✓ Field-welded piping where furnace post-weld stress relief is impractical
  • ✓ Maximum corrosion safety margin in boiling H2SO4 or concentrated HCl
  • ✓ Complex cold forming, spinning, or tube expansion

Выбирайте Zirconium 705 (UNS R60705), если

  • ✓ High-pressure ASME reactors where 85% higher yield strength cuts wall thickness
  • ✓ Zirconium fasteners, pump shafts, agitator blades, and structural internals
  • ✓ Shop-fabricated assemblies with access to vacuum or inert-gas PWHT furnaces
  • ✓ Reducing total zirconium tonnage in thick-wall pressure shells

Часто задаваемые технические вопросы

Why does ASTM B551 Zirconium 705 require post-weld stress relief when 702 does not?
The 2–3% niobium addition in Zr 705 creates high residual stresses and metastable weld-zone phases that are vulnerable to delayed hydride cracking and stress corrosion cracking in chemical service. Performing a thermal stress relief around 550–595°C restores ductility and corrosion integrity.
Does Hafnium (Hf <= 4.5%) affect chemical corrosion resistance in Zr 702 or Zr 705?
No. Industrial ASTM B551 Zr 702 and Zr 705 permit up to 4.5% hafnium, which behaves chemically almost identically to zirconium in acid service. Low-hafnium nuclear-grade zirconium (Zr-2 / Zr-4) is only needed for nuclear neutron transparency, not chemical plants.

Не уверены, какой материал подойдёт?

Сообщите применение, условия эксплуатации и бюджет — предложим оптимальную марку.

Похожие сравнения

Готовы начать свой проект?

Отправьте ваш чертёж или спецификацию, и мы ответим в течение 24 часов.

Запросить цену
Быстрый запрос
WhatsApp