Titanium (Grade 5) vs. Inconel 625
Titanium Grade 5 (Ti-6Al-4V) and Inconel 625 share comparable room-temperature tensile strength (~900 MPa), but Titanium weighs 47.5% less (4.43 g/cm³ vs. 8.44 g/cm³) and costs substantially less per unit volume, whereas Inconel 625 dominates extreme temperatures above 400°C.
| Eigenschaft | Titanium (Grade 5) | Inconel 625 |
|---|---|---|
| Dichte (g/cm³) | 4.43 ★ | 8.44 |
| Zugfestigkeit (MPa) | 895-1000 | 827-1034 |
| Max. Einsatztemperatur (°C) | 400 | 980 ★ |
| Korrosionsbeständigkeit | Excellent (seawater, oxidizing) | Sehr gut (reduzierend + oxidierend) ★ |
| Kosten pro kg (USD/kg) | $22-38 ★ | $80-150 |
| Part Weight (Equal Volume) | 47.5% lighter ★ | Baseline (1.9x heavier) |
Titanium (Grade 5) wählen, wenn
- ✓ Weight reduction is critical (subsea risers, aerospace)
- ✓ Seawater, brine, and oxidizing chloride media
- ✓ Operating temperature is below 400°C
- ✓ Reducing per-part raw material cost vs. nickel alloys
Inconel 625 wählen, wenn
- ✓ Continuous operating temperature exceeds 400–980°C
- ✓ Strong uninhibited reducing acids
- ✓ Extreme thermal creep and oxidation service
- ✓ Nuclear core or hot turbine exhaust components
Zugehörige Normen, Sorten & Produkte
Häufig gestellte technische Fragen
Why is titanium not used continuously above 450–500°C in air where Inconel 625 works?
How much lighter is a titanium subsea flange compared to Inconel 625?
Unsicher, welcher Werkstoff der richtige ist?
Nennen Sie uns Anwendung, Umgebung und Budget — wir empfehlen die passende Sorte.
Verwandte Vergleiche
Werkstoffvergleich
Titanium (Grade 5) vs. Stainless Steel (316L)
Werkstoffvergleich
Titanium (Grade 5) vs. Aluminum (7075-T6)
Werkstoffvergleich
Zirconium 702 (UNS R60702) vs. Titanium Grade 7 (Ti-0.15Pd)
Werkstoffvergleich
Titanium Grade 7 (Ti-0.15Pd) vs. Hastelloy C-276 (UNS N10276)
Werkstoffvergleich
Niobium (ASTM B393 Type 1/2) vs. Tantalum (ASTM B708)
Werkstoffvergleich
Nickel 200 (ASTM B161 / B163) vs. Titanium Grade 2 (ASTM B338)