TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) vs. Grade 5 (Ti-6Al-4V)

TA15 (Ti-6,5Al-2Zr-1Mo-1V) y el ruso GOST VT20 (ВТ20) son equivalentes metalúrgicos directos para servicio continuo a 500 °C — ampliando 150 °C la temperatura útil respecto a Ti-6Al-4V (Grado 5, máx. 350 °C) con excelente soldabilidad por fusión.

Propiedad TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) Grade 5 (Ti-6Al-4V)
Clase de aleación Near-Alpha (Ti-6.5Al-2Zr-1Mo-1V) Alpha-Beta (Ti-6Al-4V)
Equivalentes regionales TA15 (GB/T) = VT20 / ВТ20 (GOST) Grade 5 / TC4 / VT6 (ВТ6)
Temp. máx. de servicio continuo (°C) 500 (up to 3,000 hrs) ★ 300–350
Temp. pico de corta duración (°C) Up to 800 (<5 min) ★ ~400–450
Room-Temp Tensile Strength (MPa) 930–1,130 (annealed) ★ 895–1,000 (annealed)
Soldabilidad por fusión Excellent (weld efficiency >90%) ★ Good (requires strict PWHT)
High-Temp Creep Resistance Superior (Zr + Mo stabilization) ★ Moderate (<350°C)
Global Stock Availability Made-to-order / specialized mills Widely stocked globally ★

Elija TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) cuando

  • ✓ Continuous operating temperatures between 350°C and 500°C
  • ✓ Direct replacement for Russian GOST VT20 (ВТ20) forgings, plates, or bars
  • ✓ Welded aerospace engine ducts, compressor casings, and thermal bulkheads
  • ✓ High thermal creep resistance combined with >930 MPa room-temperature strength

Elija Grade 5 (Ti-6Al-4V) cuando

  • ✓ Operating temperatures stay below 350°C
  • ✓ Off-the-shelf global AMS 4928 / ASTM B348 stock and fast lead times are essential
  • ✓ Standard airframe brackets, fasteners, and CNC structural parts
  • ✓ Lowest alloy procurement cost with universal western qualification

Preguntas técnicas frecuentes

Is Chinese TA15 a direct drop-in equivalent for Russian GOST VT20 (ВТ20)?
Metallurgically yes: TA15 (Ti-6.5Al-2Zr-1Mo-1V) falls squarely within the chemical and mechanical envelope of Russian VT20 (ВТ20). Buyers replacing VT20 in flight or pressure-retaining hardware should still verify exact interstitial limits, ultrasonic class, and heat-treatment state on the Mill Test Certificate (MTC).
What is the closest Western aerospace equivalent to TA15 / VT20?
There is no 1:1 identical AMS chemistry, but Ti-6Al-2Sn-4Zr-2Mo (Ti-6242S / AMS 4919 / AMS 4976) serves a similar 450–540°C high-temperature near-alpha niche in Western gas turbine engines, though TA15/VT20 offers notably better fusion weldability.

¿No sabe qué material le conviene?

Indíquenos aplicación, entorno y presupuesto: le recomendaremos el grado óptimo.

Comparativas relacionadas

¿Listo para iniciar su proyecto?

Envíe su plano o especificación y le responderemos en un plazo de 24 horas.

Solicitar cotización
Consulta rápida
WhatsApp