Type something to search...

Zirconium 702 (UNS R60702) vs. Zirconium 705 (UNS R60705)

Bajo ASTM B551, el Circonio 705 (Zr-2,5Nb) ofrece un 85 % más de límite elástico mínimo que el Zr 702 (380 frente a 205 MPa) para paredes más delgadas a alta presión, pero exige tratamiento térmico de alivio de tensiones post-soldadura (~550–595 °C).

Propiedad Zirconium 702 (UNS R60702) Zirconium 705 (UNS R60705)
UNS y Composición R60702 (Zr+Hf >= 99.2%) R60705 (Zr + 2.0–3.0% Nb)
Min Tensile Strength (ASTM B551) (MPa) 380 (55 ksi) 550 (80 ksi) ★
Min Yield Strength (0.2%) (MPa) 205 (30 ksi) 380 (55 ksi) ★
Min Elongation (in 50 mm) (%) 16 16
Tratamiento térmico post-soldadura (PWHT) Generally not required ★ Mandatory stress relief (~550–595°C)
Corrosion Resistance (Extreme H₂SO₄) Best (unalloyed single-phase) ★ Very Good (slightly narrower ceiling)
Bend Radius / Deep Drawing Better for complex forming ★ Good (higher springback)
Typical Equipment Application Heat exchanger tubes, vessel liners, columns High-pressure reactors, shafts, bolts, pumps

Elija Zirconium 702 (UNS R60702) cuando

  • ✓ Heat exchanger tubes, distillation columns, and corrosion-resistant liners
  • ✓ Field-welded piping where furnace post-weld stress relief is impractical
  • ✓ Maximum corrosion safety margin in boiling H2SO4 or concentrated HCl
  • ✓ Complex cold forming, spinning, or tube expansion

Elija Zirconium 705 (UNS R60705) cuando

  • ✓ High-pressure ASME reactors where 85% higher yield strength cuts wall thickness
  • ✓ Zirconium fasteners, pump shafts, agitator blades, and structural internals
  • ✓ Shop-fabricated assemblies with access to vacuum or inert-gas PWHT furnaces
  • ✓ Reducing total zirconium tonnage in thick-wall pressure shells

Preguntas técnicas frecuentes

Why does ASTM B551 Zirconium 705 require post-weld stress relief when 702 does not?
The 2–3% niobium addition in Zr 705 creates high residual stresses and metastable weld-zone phases that are vulnerable to delayed hydride cracking and stress corrosion cracking in chemical service. Performing a thermal stress relief around 550–595°C restores ductility and corrosion integrity.
Does Hafnium (Hf <= 4.5%) affect chemical corrosion resistance in Zr 702 or Zr 705?
No. Industrial ASTM B551 Zr 702 and Zr 705 permit up to 4.5% hafnium, which behaves chemically almost identically to zirconium in acid service. Low-hafnium nuclear-grade zirconium (Zr-2 / Zr-4) is only needed for nuclear neutron transparency, not chemical plants.

¿No sabe qué material le conviene?

Indíquenos aplicación, entorno y presupuesto: le recomendaremos el grado óptimo.

Comparativas relacionadas

¿Listo para iniciar su proyecto?

Envíe su plano o especificación y le responderemos en un plazo de 24 horas.