Type something to search...

Grade 12 (Near-α (Ti-0.3Mo-0.8Ni)) — Properties, Specifications & Supply

Grade 12 (Ti-0.3Mo-0.8Ni, UNS R53400) is a corrosion-resistant titanium alloy designed for elevated-temperature chemical service, including NACE MR0175 sour-gas environments. It offers 483 MPa minimum tensile strength at 4.51 g/cm³ with better crevice-corrosion resistance than CP grades, and is supplied per B265, B348, B338, B381 for heat exchangers, pressure vessels and offshore oil and gas equipment.

Density

4.51 g/cm3

Melting Point

1668 °C

Tensile Strength

483–620 MPa

Yield Strength

345–483 MPa

Elastic Modulus

104 GPa

UNS Number

R53400

Chemical Composition

Ti Mo Ni Fe O C N H
Balance 0.2-0.4 0.6-0.9 ≤ 0.3 ≤ 0.25 ≤ 0.08 ≤ 0.03 ≤ 0.015

Values in wt%. Single values indicate maximum allowable content.

Mechanical Properties

Property Value Unit
Ultimate Tensile Strength 483 – 620 MPa
Yield Strength (0.2% Offset) 345 – 483 MPa
Elongation at Break ≥ 18 %
Hardness 250 HB
Elastic Modulus 104 GPa
Density 4.51 g/cm³
Melting Point 1668 °C

International Grade Equivalents

Standard Designation
ASTM (USA) Grade 12
GB/T (China) TA10
DIN/EN (Germany/EU) 3.7105
GOST (Russia) —
JIS (Japan) —
UNS (Unified) R53400

Applicable Specifications

ASTM B265 ASTM B348 ASTM B338 NACE MR0175

Request a Quote for Grade 12

We supply Grade 12 (Near-α (Ti-0.3Mo-0.8Ni)) in sheets, plates, bars, tubes, forgings, and custom forms. Certified to ASTM B265 and other applicable standards.

Get a Quote →

Frequently Asked Questions

What is Grade 12 titanium?
Grade 12 (UNS R53400, Ti-0.3Mo-0.8Ni) is a corrosion-resistant alloy specifically designed for elevated-temperature chemical service. NACE MR0175 certified for sour gas (H₂S) environments. Commonly used in heat exchangers, pressure vessels, and offshore oil & gas equipment operating up to 315°C.

Ready to Start Your Project?

Get factory-direct pricing on titanium products. No minimum order.

Get a Quote
Quick Inquiry