Titanium sheets and plates are flat-rolled mill products supplied per ASTM B265, GJB, ASME in 14 titanium grades. Sheet covers thin gauges for forming and welding; plate covers heavier sections for machining. Typical uses include heat exchangers, chemical process equipment, aerospace skins and architectural cladding, from stock and custom rolling in Baoji, China.

Sheet Thickness 0.5mm – 5.99mm
Plate Thickness 6.0mm – 100mm
Standard Sizes 1000×2000mm, 1220×2440mm (4'×8'), 1500×3000mm, 1500×6000mm, >2000×>6000mm
Surface Mill Finish (HRAP), Pickled, Sandblasted
Standards ASTM B265, GJB, ASME
Available Grades 14 grades (5 in stock)

Available Grades for Titanium Sheets & Plates

Click a grade to view its chemical composition and mechanical properties inline.

Grade 1

CPUNS: R50250GB: TA1

Softest, most formable CP titanium with best ductility. Ideal for deep drawing, welding, and chemical linings.

Full Grade Details →

Chemical Composition (wt%)

TiBalance
Fe0.20 max
O0.18 max
C0.08 max
N0.03 max
H0.015 max

Mechanical Properties

Tensile Strength240 MPa – 345 MPa
Yield Strength170 MPa – 310 MPa
Elongation (min)24%
Hardness120 HB
Elastic Modulus103 GPa

In stock, incl. elastic sheets 0.8/1.0/1.2/1.5/1.8/2.0/2.5/3.0

In-Stock Dimensions

Grade 1 (TA1)

0.5*1220*2000 0.6*1250*2780 1.0*1336*2420 1.2*1210*2530 1.3*1200*2010 1.5*1340*6000 1.6*1300*2000 1.8*1010*2420 2.0*1200*3800 2.0*1560*6000 2.5*1520*6000 3.0/4.0/5.0/6.0/8.0*1500*6000 0.5/0.6/0.8/1.0/1.2/1.5/2.0/2.5/3.0/3.5/4.0/5.0/6.0/8.0/10/12*1020*2200~3500

Grade 2 (TA2)

0.85*1294*2505 1.6*1270*2005 3.0/4.0/5.0/6.0/8.0/10.0/12.0/20/22/25/30/35*1500*6000 6/8/12/14/16/18/20/22/24/25/26/28/30/32/35/40/45/48/50/55/60/65*>2000*>6000 0.8/1.0/1.5/2.0/2.5/3.0/4.0/4.5/5.0/6.0/6.5/7.0/8.0/10/12*1020*2200 1.0*1000*2500 8.0/10/12/14/15/16/18/20/22/25/26/28/30/32/35/40/45/50/55/60/65/80*1500*6000

Grade 4 (TA3)

0.5/0.8/1.0/1.3/1.5/1.7/2.0/2.5/3.0*1000*2000

Grade 5 (TC4)

6*1500*6000 8*2000*6000 10*2000*6000 0.8/1.0/1.2/1.5/2.0/2.5/3.0/4.0/5.0/6.0/8.0/10/12/14/15/16/18/20/25/30/35/40/45/50/55/60*1020*2200 20/25/35/40/55/65*cut-to-size

Grade 12 (TA10)

0.8*1270*2440 1.0*1150*3000 1.5*1000*2000 2.0*1020*2250 3.0/4.0/5.0/6.0/8.0/10.0/12*1500*6000 8.0/10/12/14/16/18/20/25/30/50*>2000*>6000 0.7*1220*2440 6.0/8.0/10/12/14/16/18/20/25/30/35/40*1500*in stock

Titanium Sheets & Plates Weight Calculator

Calculated Weight

Per piece44.300 kg
Imperial97.665 lbs

Cost Estimate (FOB Baoji)

Price tierPrototype / R&D
Unit price$86.4/kg
Estimated total$3,827.52

* Reference pricing only. Actual quote depends on specifications, tolerances, and certification requirements.

Grade 5 Properties

Density4.43 g/cm³Tensile895–1000 MPaYield828–910 MPaElongation10%
Request Quote for This Specification →

Quality & Certification

📋

Material Test Certificate

EN 10204 Type 3.1/3.2 MTC with every shipment. Full heat traceability.

🔬

Testing & Inspection

UT, PMI, tensile test, hardness test. Third-party inspection available.

✅

Standards Compliance

Supplied to ASTM / ASME / AMS / GJB as specified. Approval scope confirmed per order.

🚚

Fast Delivery

Stock items: 3 days. Custom orders: 15–45 days. FOB Baoji / CIF worldwide.

Technical Guide: Titanium Sheets & Plates

Titanium Sheets & Plates

An Introduction to Versatile Titanium Sheets & Plates

Titanium sheets and plates are the foundational forms of titanium, representing one of the most versatile and widely used product types in the industry. Produced by hot and cold rolling slabs into flat products, they are differentiated by thickness: “sheet” typically refers to material under 6.0 mm thick, while “plate” refers to material 6.0 mm and thicker.

These products serve as the starting point for countless fabrication projects, offering an unparalleled combination of high strength-to-weight ratio, exceptional corrosion immunity, and excellent durability. Whether being laser-cut for intricate parts, formed into pressure vessels, or welded into large-scale structures, titanium sheets and plates provide the raw material for innovation in the world’s most demanding engineering fields.


Available Dimensions & Specifications

We stock a comprehensive inventory of titanium sheets and plates to meet a wide range of industrial and commercial needs.

  • Thickness:
    • Sheet: 0.5 mm to 5.99 mm (0.020” to 0.236”)
    • Plate: 6.0 mm to 100 mm (0.236” to 4.0”)
  • Standard Sizes:
    • 1000mm x 2000mm
    • 1220mm x 2440mm (4 ft x 8 ft)
    • 1500mm x 3000mm
  • Surface Finish: Standard Mill Finish (No. 1 / HRAP), Pickled, or Sandblasted.
  • Standards: Primarily manufactured to ASTM B265 specifications.
  • Services: Custom laser, waterjet, or plasma cutting available to your specifications.

Common Titanium Sheet & Plate Grades

The selection of a specific grade is determined by the application’s requirements for strength, formability, and corrosion resistance.

GradeCommon Name(s)Key Characteristics & FeaturesTypical Sheet & Plate Applications
Grade 2CP Ti Grade 2The most widely used grade. Offers excellent balance of moderate strength, good formability, and outstanding corrosion resistance.Chemical processing tanks, pressure vessels, heat exchanger plates, architectural cladding, piping systems.
Grade 5Ti-6Al-4VThe “workhorse” titanium alloy. Very high strength, good fatigue resistance. More difficult to form than CP grades.Aerospace structural components (wings, fuselage), armor plating, high-performance motorsport chassis parts.
Grade 1CP Ti Grade 1The softest and most ductile grade. Provides the best formability for complex or deep-drawing applications.Plate-and-frame heat exchangers, expanded metal anodes, applications requiring extreme forming.
Grade 7Ti-0.2PdMechanically identical to Grade 2, but with palladium added for enhanced corrosion resistance, especially against crevice corrosion.Linings for highly corrosive chemical vessels, specialized desalination equipment, and process piping.
Grade 12Ti-0.3Mo-0.8Ni”Near-alpha” alloy with enhanced high-temperature strength and superior crevice corrosion resistance compared to CP grades.Heat exchangers in higher temperature/mildly reducing environments, chemical processing equipment.

Example Applications of Titanium Sheets & Plates

The robust and reliable nature of titanium plates and sheets makes them a cornerstone material across numerous industries.

Aerospace & Defense

  • Airframe Structures: Used for fuselage skins, wing structures, bulkheads, and engine nacelles where weight reduction and strength are paramount.
  • Armor Plating: Titanium plate offers excellent ballistic protection at a lower weight than steel, used in military vehicles and personal protection.
  • Engine Components: Formed and fabricated into parts for jet engines that must withstand high temperatures and stress.

Chemical Processing & Energy

  • Pressure Vessels & Tanks: The superior corrosion resistance makes titanium ideal for storing and processing aggressive chemicals, acids, and chlorides.
  • Plate Heat Exchangers: Thin titanium sheets are corrugated and stacked to create highly efficient and corrosion-proof heat transfer units.
  • Desalination Plants: Extensively used for piping, vessels, and heat exchangers that are in constant contact with saltwater.

Marine & Offshore

  • Shipbuilding: Used for hull plates on high-speed naval vessels, submarine components, and offshore platform risers and piping.
  • Ballast Water Systems: Provides a long-term, maintenance-free solution for piping and valves exposed to corrosive seawater.

Architecture & Construction

  • Façades and Roofing: Creates iconic, long-lasting building exteriors that are lightweight and impervious to pollution and acid rain (e.g., Guggenheim Museum Bilbao).
  • Sculptures and Monuments: Chosen by artists for its durability, unique luster, and ability to be anodized into different colors.

Related News & Insights

Ready to Start Your Project?

Get factory-direct pricing on titanium products. No minimum order.

Get a Quote
Quick Inquiry