Grade 23 (α+β ELI (Ti-6Al-4V ELI)) — Properties, Specifications & Supply

Grade 23 (Ti-6Al-4V ELI, UNS R56407) is the extra-low-interstitials version of Grade 5, with oxygen capped at 0.13% for superior fracture toughness and biocompatibility. It delivers 828 MPa minimum tensile strength at 4.43 g/cm³ and is supplied per F136 — the mandatory chemistry for orthopedic implants, spinal devices and fracture-critical aerospace parts.

Density

4.43 g/cm3

Melting Point

1660 °C

Tensile Strength

828–965 MPa

Yield Strength

759–869 MPa

Elastic Modulus

114 GPa

UNS Number

R56407

Chemical Composition

Ti Al V Fe O C N H
Balance 5.5-6.5 3.5-4.5 ≤ 0.25 ≤ 0.13 ≤ 0.08 ≤ 0.05 ≤ 0.012

Values in wt%. Single values indicate maximum allowable content.

Mechanical Properties

Property Value Unit
Ultimate Tensile Strength 828 – 965 MPa
Yield Strength (0.2% Offset) 759 – 869 MPa
Elongation at Break ≥ 10 %
Hardness 320 HB
Elastic Modulus 114 GPa
Density 4.43 g/cm³
Melting Point 1660 °C

International Grade Equivalents

Standard Designation
ASTM (USA) Grade 23
GB/T (China) TC4 ELI
DIN/EN (Germany/EU) 3.7165-ELI
GOST (Russia) ВТ6С
JIS (Japan) —
UNS (Unified) R56407

Applicable Specifications

ASTM F136 ISO 5832-3

Request a Quote for Grade 23

We supply Grade 23 (α+β ELI (Ti-6Al-4V ELI)) in sheets, plates, bars, tubes, forgings, and custom forms. Certified to ASTM F136 and other applicable standards.

Get a Quote →

Frequently Asked Questions

What is Grade 23 titanium?
Grade 23 (Ti-6Al-4V ELI, UNS R56407) is the medical-grade version of Grade 5. 'ELI' means Extra Low Interstitials — oxygen capped at 0.13% (vs 0.20% in Grade 5). This improves fracture toughness and biocompatibility. Mandatory per ASTM F136 / ISO 5832-3 for orthopedic implants, spinal devices, and dental fixtures.
Can Grade 23 be used in aerospace?
Yes. Beyond medical implants, Grade 23 is specified for fracture-critical aerospace parts — components where a crack would be catastrophic (e.g., rotor hubs, high-cycle fatigue brackets). The ELI chemistry provides a measurable improvement in fatigue crack growth resistance.

Ready to Start Your Project?

Get factory-direct pricing on titanium products. No minimum order.

Get a Quote
Quick Inquiry