Type something to search...
📦 Looking for Titanium Wires specs, grades & pricing?
View Full Product Page →
TB13 Beta Titanium Wire for Premium Eyewear Frames

TB13 Beta Titanium Wire for Premium Eyewear Frames

TB13 Beta Titanium Wire for Eyewear Temples & Bridges

TB13 is a Chinese metastable beta titanium alloy (GB/T 3620.1) used for eyewear frames, temples and bridges. Like other beta titanium alloys, it combines a lower elastic modulus than commercially pure titanium or Ti-6Al-4V with good cold formability — the reason beta alloys are chosen for flexible temples that spring back after bending.

For many frame makers the question is not whether TB13 works, but whether a Chinese-made wire behaves like the imported wire already qualified on their lines. The data below answers that directly.


Side-by-Side Test: Partner-Mill TB13 vs Italian Reference Wire

The partner mill tested its TB13 wire against an Italian-made reference wire under the same conditions:

PropertyItalian reference wirePartner-mill TB13 wire
Tensile strength, Rm (MPa)736722
Yield strength, Rp0.2 (MPa)713702
Elongation, A (%)3232.5
Reduction of area, Z (%)6467
Hardness (HV, three points)230 / 232 / 230224 / 227 / 227
Grain size, transverse11.2 µm22.5 µm
Grain size, longitudinal22.5 µm22.5 µm

What the table shows:

  • Strength is within about 2% of the Italian wire.
  • Ductility — elongation and reduction of area — is equal or slightly higher, which matters for temple bending and rim-wire rolling.
  • Grain size is the same longitudinally; the Italian wire has a finer transverse grain. If your process is sensitive to grain size, specify it in the purchase order.

These are the mill’s own test results on the supplied condition, not an independent laboratory report. Results for your order are reported on the MTC, and third-party re-testing can be arranged.


Ordering

  • Diameter, coil or straight lengths, and surface finish are quoted against your drawing.
  • Strength can be increased by ageing after forming; if you need aged properties, state the target and heat-treatment route so the test plan can be agreed.
  • Documents: each lot is supplied with a material test certificate showing chemistry and mechanical results.

Request a Quote for This Product

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Contact

Reply within 24 hours 🔒 NDA available on request — your drawings stay confidential 📦 Small quantities ship as LCL; larger orders ship as full containers for simpler loading and customs inspection.

WhatsApp
Quality Assurance
  • ✓ Material Test Certificate (MTC) with Every Order
  • ✓ ASTM / ASME / AMS Standard Compliance
  • ✓ Third-party Inspection Available
Request MTC / Test Report
Related Products

Ready to Start Your Project?

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Inquiry
WhatsApp