AMS 4914 — Titanium Alloy Sheet and Strip, 15V - 3.0Cr - 3.0Sn - 3.0Al (TB5 / Ti-15-3), Solution Heat Treated
SAE AMS 4914 governs solution-heat-treated metastable beta titanium Ti-15V-3Cr-3Sn-3Al (Chinese TB5 / UNS R58153) strip, sheet, and foil engineered for severe room-temperature cold forming followed by low-temperature aging (482–538°C) to exceed 1,100–1,250 MPa tensile strength.
Scope
Covers cold-rolled metastable beta titanium alloy Ti-15V-3Cr-3Sn-3Al (TB5) in sheet, strip, and foil form delivered in the solution-heat-treated condition for aerospace ducting, honeycomb cores, bellows, and high-strength formed parts.
Covered Grades
Covered Product Forms
Key Requirements
- Nominal chemistry: 14–16% V, 2.5–3.5% Cr, 2.5–3.5% Sn, 2.5–3.5% Al
- Delivered solution-treated (790–815°C) for tight room-temperature bend radius (~2T)
- Age-hardenability verification (482–538°C aging boosts UTS to >1,100–1,250 MPa)
- 100% freedom from alpha-case and strict thickness/flatness control
Test Methods
- ASTM E8 (Tensile — ST & Aged)
- ASTM E290 (Bend Testing)
- ASTM E1409 (Oxygen/Nitrogen)
- AMS 2242 (Tolerances)
Metallurgical Verification & Quality Control
Unlike Grade 5 (Ti-6Al-4V) which requires expensive hot-forming above 700°C for complex shapes, AMS 4914 (TB5) can be cold-stamped, deep-drawn, and welded at room temperature in the solution-treated BCC beta phase, then vacuum-aged to aerospace strength levels.
What to Specify on Your AMS 4914 Purchase Order / RFQ
- Standard & alloy: AMS 4914 (Ti-15V-3Cr-3Sn-3Al / TB5 / UNS R58153)
- Delivery condition: Solution Heat Treated (ST) ready for cold forming (plus coupon aging test verification)
- Gauge & form: foil/strip (0.05–1.0 mm) or sheet up to 3.2 mm, coil ID or cut-to-length sheets
- Bend radius requirement and surface finish (bright vacuum-annealed or pickled)
- Certification: aerospace MTC documenting both ST and aged coupon tensile/yield results
Code Equivalency & Companion Standards
Directly equivalent to GB/T TB5 cold-rolled strip/foil. Compare against AMS 4911 (Ti-6Al-4V) when room-temperature stamping or tight bend radii rule out alpha-beta sheets.
AMS 4914 Specification & Procurement FAQ
What does AMS 4914 cover and which product forms are included?
Which titanium grades are covered under AMS 4914?
What testing and inspection methods are required by AMS 4914?
Related Specifications
Need material certified to AMS 4914?
Tell us grade, product form, and dimensions. We quote with a material test certificate (MTC) compliant with AMS 4914; the applicable standard edition and approvals are stated on the quotation. Quote within 24 hours.