ASTM F67 — Standard Specification for Unalloyed Titanium, for Surgical Implant Applications (UNS R50250, UNS R50400, UNS R50550, UNS R50700)
ASTM F67 covers the chemical, mechanical, and metallurgical requirements for four grades of unalloyed commercially pure titanium (Grades 1, 2, 3, and 4) used in surgical, dental, and maxillofacial implants.
Scope
Covers the chemical, mechanical, and metallurgical requirements for four grades of unalloyed titanium (Grades 1, 2, 3, and 4) used in the manufacture of surgical implants.
Covered Product Forms
Key Requirements
- Unalloyed titanium chemistry with step-wise oxygen limits from Grade 1 (0.18% max) to Grade 4 (0.40% max)
- Minimum tensile strength ranging from 240 MPa (Gr1) to 550 MPa (Gr4 annealed)
- Equiaxed alpha grain size no coarser than ASTM E112 No. 5
- Bend test compliance for flat sheet and strip
Test Methods
- ASTM E8 (Tensile)
- ASTM E1409 (Inert Gas Fusion)
- ASTM E290 (Bend Testing)
- ASTM E112 (Grain Size)
Metallurgical Verification & Quality Control
Within ASTM F67, Grade 1 offers the highest ductility for cranial plates and maxillofacial mesh, whereas Grade 4 (and cold-worked Grade 4) delivers the highest strength of unalloyed titanium—making it the global standard for vanadium-free and aluminum-free dental implants.
What to Specify on Your ASTM F67 Purchase Order / RFQ
- Standard and grade: ASTM F67 Grade 1, Grade 2, Grade 3, or Grade 4 (and ISO 5832-2 if required)
- Condition: annealed or cold-worked (specify target minimum UTS if ordering cold-worked Grade 4 dental bar)
- Form, dimensions, and precision tolerance (e.g., h6/h7 ground bar for dental CNC turning or thin sheet for bone plates)
- Grain size and ultrasonic inspection requirements
- Certification: material test certificate (MTC) with ASTM E112 grain size rating, chemical/gas analysis, and tensile test report
Code Equivalency & Companion Standards
ASTM F67 corresponds to ISO 5832-2. When higher yield strength (>790 MPa) is required for load-bearing orthopedic joints and spine hardware, specify ASTM F136 (Grade 23 Ti-6Al-4V ELI).
ASTM F67 Specification & Procurement FAQ
What does ASTM F67 cover and which product forms are included?
Which titanium grades are covered under ASTM F67?
What testing and inspection methods are required by ASTM F67?
Related Specifications
Need material certified to ASTM F67?
Tell us grade, product form, and dimensions. We quote with a material test certificate (MTC) compliant with ASTM F67; the applicable standard edition and approvals are stated on the quotation. Quote within 24 hours.