Rolls-Royce Orders Additively Manufactured Ti-6Al-4V Engine Parts from Norsk Titanium
Rolls-Royce places purchase order with Norsk Titanium for wire-DED additive Ti-6Al-4V aerospace components, cutting buy-to-fly ratios and lead times.