Scope
Covers nickel (UNS N02200) and low-carbon nickel (UNS N02201) in the form of cold-worked or hot-worked seamless pipe and tube for corrosive chemical piping.
Covered Grades
Covered Product Forms
Key Requirements
- Ni min 99.0%; Carbon max 0.15% (Ni 200) vs max 0.02% (Ni 201 for >315°C)
- Annealed min tensile 380 MPa / yield 103 MPa (Ni 200, <=127 mm OD)
- Hydrostatic or non-destructive electric testing on every pipe
- Dimensioned per NPS/Schedule (ASME B36.19M) or custom OD × WT
Test Methods
- ASTM E8 (Tensile)
- ASTM E1473 (Chemical Analysis)
- ASTM E213 / E571 (NDT)
Metallurgical Verification & Quality Control
Specify ASTM B161 Nickel 200 for hot 30–73% caustic soda (NaOH) transfer piping below 315°C—where titanium suffers hydride embrittlement. For service above 315°C (600°F), switch to low-carbon Nickel 201 (UNS N02201) to prevent intergranular graphitization.
What to Specify on Your ASTM B161 Purchase Order / RFQ
- Standard & grade: ASTM B161 / ASME SB-161 UNS N02200 (Ni 200) or N02201 (Ni 201)
- Condition: annealed (standard for welding/bending) or stress-relieved
- Size: NPS & Schedule (e.g., 2" Sch 40S) or exact OD × wall thickness × length
- End finish: plain ends or beveled ends for butt welding
- Certification: EN 10204 3.1 MTC with chemical carbon check, tensile test, and hydro/NDT report
Code Equivalency & Companion Standards
ASME SB-161 covers piping in ASME B31.3 and Section VIII. For heat-exchanger and caustic-evaporator condenser tubing requiring tighter tolerances, specify ASTM B163.
ASTM B161 Specification & Procurement FAQ
What does ASTM B161 cover and which product forms are included?
Which nickel grades are covered under ASTM B161?
What testing and inspection methods are required by ASTM B161?
Related Specifications
Need material certified to ASTM B161?
Tell us grade, product form, and dimensions. We quote with a material test certificate (MTC) compliant with ASTM B161; the applicable standard edition and approvals are stated on the quotation. Quote within 24 hours.