Type something to search...
ASTM Standard

ASTM B163 — Standard Specification for Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tubes

ASTM B163 (ASME SB-163) covers seamless cold-worked and annealed Nickel 200/201 condenser and heat-exchanger tubes (up to 3 in. / 76.2 mm OD) engineered for chlor-alkali caustic soda evaporators and high-conductivity alkaline heat transfer.

Scope

Covers seamless tubes of nickel and nickel alloys (including UNS N02200 and N02201) for use in surface condensers, evaporators, and heat exchangers.

Covered Grades

Nickel 200 (UNS N02200) Nickel 201 (UNS N02201)

Covered Product Forms

Seamless Tube

Key Requirements

  • Tighter OD, wall thickness, and straightness tolerances for tubesheet expansion
  • Mandatory flaring test, flattening test, and grain-size control
  • 100% hydrostatic or pneumatic-under-water plus eddy-current NDT
  • High thermal conductivity (~70 W/m·K) for falling-film NaOH evaporators

Test Methods

  • ASTM E8 (Tensile)
  • ASTM E571 (Eddy Current)
  • ASTM E112 (Grain Size)
  • ASTM E1473 (Chemistry)

Metallurgical Verification & Quality Control

While ASTM B161 governs general nickel piping, ASTM B163 is mandatory for caustic soda falling-film evaporator tube bundles where precise OD/wall control, flare ductility for tubesheet rolling, and 100% leak verification are essential.

What to Specify on Your ASTM B163 Purchase Order / RFQ

  • Standard & grade: ASTM B163 / ASME SB-163 UNS N02200 (Ni 200) or N02201 (Ni 201)
  • Condition: annealed (bright annealed or pickled) or stress-relieved (specify for U-bends)
  • Exact OD × minimum wall thickness × straight length (or U-bend radius drawing)
  • Testing: 100% eddy-current (ET) + hydrostatic/pneumatic test + flare/flattening coupon tests
  • Certification: EN 10204 3.1 / 3.2 MTC with heat traceability and full NDT records

Code Equivalency & Companion Standards

Adopted as ASME SB-163 for Section VIII heat exchangers. Pair with ASTM B338 titanium tubes on the brine/chlorine side of chlor-alkali plants.

ASTM B163 Specification & Procurement FAQ

What does ASTM B163 cover and which product forms are included?
ASTM B163 (Standard Specification for Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tubes) covers seamless tubes of nickel and nickel alloys (including UNS N02200 and N02201) for use in surface condensers, evaporators, and heat exchangers. Covered product forms include Seamless Tube.
Which nickel grades are covered under ASTM B163?
ASTM B163 covers Nickel 200 (UNS N02200), Nickel 201 (UNS N02201). Every batch supplied by Titanium Seller under ASTM B163 ships with a material test certificate with heat/lot number traceability.
What testing and inspection methods are required by ASTM B163?
Key compliance requirements for ASTM B163 include tighter od, wall thickness, and straightness tolerances for tubesheet expansion, mandatory flaring test, flattening test, and grain-size control, 100% hydrostatic or pneumatic-under-water plus eddy-current ndt, high thermal conductivity (~70 w/m·k) for falling-film naoh evaporators, verified using standard test methods: ASTM E8 (Tensile), ASTM E571 (Eddy Current), ASTM E112 (Grain Size), ASTM E1473 (Chemistry).

Need material certified to ASTM B163?

Tell us grade, product form, and dimensions. We quote with a material test certificate (MTC) compliant with ASTM B163; the applicable standard edition and approvals are stated on the quotation. Quote within 24 hours.

Ready to Start Your Project?

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Inquiry
WhatsApp