ASTM B393 — Standard Specification for Niobium and Niobium Alloy Strip, Sheet, and Plate
ASTM B393 covers four grades of wrought niobium strip, sheet, and plate—reactor and commercial unalloyed niobium (Types 1 & 2) plus Nb-1%Zr alloys (Types 3 & 4)—offering half the density of tantalum (8.57 g/cm³) for corrosion liners and high-voltage anode substrates.
Scope
Covers unalloyed niobium (UNS R04200, R04210) and niobium-1% zirconium alloy (UNS R04251, R04261) strip, sheet, and plate in annealed or cold-worked conditions.
Covered Grades
Covered Product Forms
Key Requirements
- Strict interstitial gas ceilings (O, N, C, H) to preserve room-temperature ductility
- Type 1/2: unalloyed Nb (min 99.85–99.9%); Type 3/4: 0.8–1.2% Zr for high-temp strength
- Recrystallized annealed condition for deep drawing and vessel lining
- Surface clean, uniform, and free of oxide scale or laminations
Test Methods
- ASTM E8 (Tensile)
- ASTM E1409 (Inert Gas Fusion)
- ASTM E29 (Rounding)
Metallurgical Verification & Quality Control
Commercial ASTM B393 Type 2 (UNS R04210) is the standard selection for platinized high-voltage cathodic protection anodes (>40 V breakdown in chlorides) and moderate nitric/HCl chemical liners. Specify Type 3/4 (Nb-1Zr) for elevated-temperature vacuum furnace or aerospace hardware.
What to Specify on Your ASTM B393 Purchase Order / RFQ
- Standard & type: ASTM B393 Type 1 (R04200), Type 2 (R04210), Type 3 (R04251), or Type 4 (R04261)
- Temper condition: fully recrystallized annealed (standard) or stress-relieved / cold-worked
- Gauge, width, length, and surface finish (bright vacuum-annealed or pickled)
- Special chemistry controls (e.g., max Tantalum ppm for superconducting / RRR applications)
- Certification: EN 10204 3.1 MTC with chemical impurities, interstitials, and tensile elongation
Code Equivalency & Companion Standards
Complements ASTM B392 (niobium bar, rod, and wire) and ASTM B394 (seamless and welded niobium tubes). Evaluate against Tantalum (ASTM B708) when boiling concentrated HCl/H2SO4 is present.
ASTM B393 Specification & Procurement FAQ
What does ASTM B393 cover and which product forms are included?
Which niobium grades are covered under ASTM B393?
What testing and inspection methods are required by ASTM B393?
Related Specifications
Need material certified to ASTM B393?
Tell us grade, product form, and dimensions. We quote with a material test certificate (MTC) compliant with ASTM B393; the applicable standard edition and approvals are stated on the quotation. Quote within 24 hours.