ASTM B551 — Standard Specification for Zirconium and Zirconium Alloy Strip, Sheet, and Plate
ASTM B551 (ASME SB-551) governs annealed zirconium and zirconium-alloy strip, sheet, and plate—primarily commercially pure Grade 702 (UNS R60702) and higher-strength Zr-2.5%Nb Grade 705 (UNS R60705)—for hydrochloric, sulfuric, and acetic acid process equipment.
Scope
Covers four grades of wrought zirconium and zirconium-alloy strip, sheet, and plate (Grades R60702, R60704, R60705, and R60706) for corrosion-resistant chemical processing and pressure vessels.
Covered Grades
Covered Product Forms
Key Requirements
- Zr+Hf min 99.2% for R60702; 2.0–3.0% Nb for R60705 (Hf max 4.5%)
- Minimum tensile/yield: 380/205 MPa (Zr 702) vs 550/380 MPa (Zr 705)
- Bend test compliance and surface freedom from scale/alpha-case
- Mandatory post-weld stress relief (~550–595°C) required for welded Zr 705 equipment
Test Methods
- ASTM E8 (Tensile)
- ASTM E290 (Bend Testing)
- ASTM E1409 (Oxygen/Nitrogen)
- ASTM E1447 (Hydrogen)
Metallurgical Verification & Quality Control
Choose ASTM B551 R60702 for boiling 0–37% HCl and up to 70% H2SO4 vessels where straightforward as-welded fabrication is preferred; choose R60705 when ASME Section VIII pressure shells benefit from 85% higher yield strength and shop PWHT furnace capacity is available.
What to Specify on Your ASTM B551 Purchase Order / RFQ
- Standard & UNS grade: ASTM B551 / ASME SB-551 Grade R60702 (Zr 702) or R60705 (Zr 705)
- Dimensions: thickness, width, length, and flatness tolerance
- Surface finish: cold-rolled pickled, vacuum annealed, or blast-and-pickled plate
- Inspection: ultrasonic testing (UT) for thick vessel plates or clad backing plates
- Certification: EN 10204 3.1 / 3.2 MTC with full chemistry (incl. Hf, Fe+Cr, O, H) and tensile/bend values
Code Equivalency & Companion Standards
Adopted by ASME as SB-551 for Section VIII Division 1 pressure vessels. Compare Zr 702 vs Zr 705 or Zr 702 vs Titanium Grade 7 before locking vessel material.
ASTM B551 Specification & Procurement FAQ
What does ASTM B551 cover and which product forms are included?
Which zirconium grades are covered under ASTM B551?
What testing and inspection methods are required by ASTM B551?
Related Specifications
Need material certified to ASTM B551?
Tell us grade, product form, and dimensions. We quote with a material test certificate (MTC) compliant with ASTM B551; the applicable standard edition and approvals are stated on the quotation. Quote within 24 hours.