PyroGenesis Secures Major Aerospace Ti-6Al-4V Powder Contract: How DED Unblocks Forging Lead Times
Examine PyroGenesis's November 2026 contract for coarse Ti-6Al-4V powder (45–150 μm), comparing DED vs. LPBF, feedstock purity, and paths to bypass forging bottlenecks.