Type something to search...

Titanium (Grade 5) vs Inconel 625 — Complete Comparison

Property Titanium (Grade 5) Inconel 625
Density (g/cm³) 4.43 ★ 8.44
Tensile Strength (MPa) 895-1000 827-1034
Max Service Temp (°C) 400 980 ★
Corrosion Resistance Excellent (oxidizing) Excellent (reducing + oxidizing) ★
Cost per kg (USD/kg) $42-65 ★ $80-150
Weight 45% lighter ★ Baseline

Choose Titanium (Grade 5) When

  • ✓ Weight is critical
  • ✓ Oxidizing environments
  • ✓ Cost-sensitive but need corrosion resistance
  • ✓ Operating below 400°C

Choose Inconel 625 When

  • ✓ High temperature > 400°C required
  • ✓ Reducing acid environments
  • ✓ Combined high temp + corrosion
  • ✓ Nuclear or extreme chemical exposure

Not sure which material is right for your project?

Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.

Related Comparisons

Ready to Start Your Project?

Get factory-direct pricing on titanium products. No minimum order.

Get a Quote
Quick Inquiry
WhatsApp