Nickel 200 (ASTM B161 / B163) vs Titanium Grade 2 (ASTM B338) — Complete Comparison
In hot concentrated caustic soda (NaOH >30% above 80–100°C), Nickel 200 (UNS N02200, ASTM B161/B163) is the mandatory industry standard with corrosion rates below 0.025 mm/yr, whereas Titanium Grade 2 suffers accelerated dissolution and severe hydride embrittlement in hot strong alkalis despite dominating the chlorine/brine side of the same chlor-alkali plant.
| Property | Nickel 200 (ASTM B161 / B163) | Titanium Grade 2 (ASTM B338) |
|---|---|---|
| UNS & Tube Spec | N02200 (ASTM B161 / B163) | R50400 (ASTM B338 / B861) |
| Hot Caustic Soda (50% NaOH, >100°C) | Excellent (<0.025 mm/yr) ★ | Poor — hydride embrittlement & corrosion |
| Wet Chlorine / Hot Chloride Brine | Poor — rapid pitting/attack | Excellent (immune <80°C; Gr7 >100°C) ★ |
| Thermal Conductivity (W/m·K) | 70.2 ★ | 21.9 |
| Density (g/cm³) | 8.89 | 4.51 ★ |
| Tensile / Yield Strength (Annealed) (MPa) | 380 / 103 (min) | 345 / 275 (min) ★ |
| Max Continuous Service Temp (°C) | 315 (use Ni 201 >315°C) | 315 (ASME pressure vessels) |
| Primary Chlor-Alkali Role | Caustic evaporators & NaOH heaters | Brine heaters, wet Cl₂ coolers, anodes |
Choose Nickel 200 (ASTM B161 / B163) When
- ✓ 30–73% caustic soda (NaOH) or potassium hydroxide (KOH) evaporators above 80°C
- ✓ High heat-transfer efficiency needed in alkaline falling-film evaporators
- ✓ Synthetic fiber, food-grade caustic, and alkaline battery precursor reactors
- ✓ ASTM B163 condenser tubes or ASTM B161 caustic transfer piping
Choose Titanium Grade 2 (ASTM B338) When
- ✓ Seawater, concentrated NaCl brine heaters, and desalination condensers
- ✓ Wet chlorine gas coolers, hypochlorites, and oxidizing acid streams
- ✓ Weight-sensitive heat exchangers requiring 49% lower tube bundle mass
- ✓ Neutral or mildly alkaline media (<10% NaOH below 60°C)
Engineering Trade-Off Analysis: Nickel 200 (ASTM B161 / B163) vs. Titanium Grade 2 (ASTM B338)
The Chlor-Alkali Plant Split (Why Both Metals Coexist): Every modern membrane chlor-alkali plant requires both metals in adjacent loops. On the anolyte/wet-chlorine/brine side (acidic oxidizing chlorides), Nickel 200 corrodes rapidly while Titanium Grade 2 and Grade 7 are completely immune. On the catholyte/caustic evaporator side (32% to 50%+ NaOH at 100–180°C), strong OH⁻ ions dissolve titanium's TiO2 film and drive atomic hydrogen into the metal lattice, causing brittle failure—making Nickel 200 (or low-carbon Nickel 201 above 315°C) essential.
ASTM B161 vs. ASTM B163 Selection for Nickel 200: For process transfer piping ordered by Nominal Pipe Size (NPS) and Schedule, specify ASTM B161 seamless nickel pipe. For falling-film caustic evaporator tubes and shell-and-tube heat exchangers ordered by exact OD and wall thickness, specify ASTM B163 seamless condenser and heat-exchanger tubes.
Thermal Conductivity & Graphitization Limit (315°C): Commercially pure Nickel 200 delivers roughly 3× the thermal conductivity of Grade 2 titanium (~70 W/m·K vs. ~22 W/m·K), enabling compact caustic evaporator tube bundles. Note that above 315°C (600°F), Nickel 200 can suffer intergranular graphitization, so Nickel 201 (C <= 0.02%) must be specified for molten caustic concentrators.
Related Specifications, Grades & Mill Products
Frequently Asked Questions: Nickel 200 (ASTM B161 / B163) vs Titanium Grade 2 (ASTM B338)
What is the difference between ASTM B161 and ASTM B163 for Nickel 200 tubes?
Why does Titanium Grade 2 fail in hot concentrated sodium hydroxide (NaOH)?
Not sure which material is right for your project?
Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.
Related Comparisons
Material Comparison
Titanium (Grade 5) vs Stainless Steel (316L)
Material Comparison
Titanium (Grade 5) vs Aluminum (7075-T6)
Material Comparison
Titanium (Grade 5) vs Inconel 625
Material Comparison
Zirconium 702 (UNS R60702) vs Titanium Grade 7 (Ti-0.15Pd)
Material Comparison
Titanium Grade 7 (Ti-0.15Pd) vs Hastelloy C-276 (UNS N10276)
Material Comparison
Niobium (ASTM B393 Type 1/2) vs Tantalum (ASTM B708)