Type something to search...

Zirconium 702 (UNS R60702) vs Titanium Grade 7 (Ti-0.15Pd) — Complete Comparison

Zirconium 702 (UNS R60702) withstands all concentrations of pure hydrochloric acid (0–37% HCl) above its boiling point (>130°C) at <0.05 mm/yr corrosion rate, whereas Titanium Grade 7 (Ti-0.15Pd, UNS R52400) is limited to dilute/moderate HCl but tolerates oxidizing impurities (Fe³⁺, Cu²⁺, wet chlorine) that rapidly pit zirconium.

Property Zirconium 702 (UNS R60702) Titanium Grade 7 (Ti-0.15Pd)
UNS & Standard R60702 (ASTM B551 / B523 / B550) R52400 (ASTM B265 / B338 / B348)
Density (g/cm³) 6.51 4.51 ★
Pure HCl Resistance All conc. (0–37%) above boiling (>130°C) ★ Dilute/moderate (<10–20% depending on temp)
Sensitivity to Fe³⁺ / Cu²⁺ / Wet Cl₂ High risk — causes rapid pitting in HCl Immune — oxidizing ions stabilize TiO2 ★
Sulfuric Acid (H₂SO₄) Limit Up to 70% at boiling point ★ Dilute (<10% boiling) or inhibited streams
Hydrofluoric Acid (HF) Resistance Destroyed by trace fluorides Destroyed by trace fluorides
Tensile / Yield Strength (Min) (MPa) 380 / 205 345 / 275
Relative Volume Cost Higher (higher density + Zr sponge) Lower (weldable to Gr2 shell; Pd-driven) ★

Choose Zirconium 702 (UNS R60702) When

  • ✓ Boiling or superheated concentrated HCl (10–37%) or 50–70% H2SO4
  • ✓ Acetic acid, formic acid, and urea synthesis heat exchangers
  • ✓ Process stream is strictly free of Fe³⁺, Cu²⁺, and free wet chlorine
  • ✓ Zero-corrosion lining or reactor tubing in strongly reducing acids

Choose Titanium Grade 7 (Ti-0.15Pd) When

  • ✓ Hot chloride brines, seawater evaporators, and crevice-prone tubesheets
  • ✓ Mixed acid streams containing Fe³⁺, Cu²⁺, nitrates, or wet chlorine gas
  • ✓ Dilute reducing acid pockets where Grade 2 suffers crevice attack
  • ✓ Welding corrosion-resistant nozzles directly to Grade 2 titanium vessels

Engineering Trade-Off Analysis: Zirconium 702 (UNS R60702) vs. Titanium Grade 7 (Ti-0.15Pd)

Hydrochloric & Sulfuric Acid Envelope: Unalloyed Zirconium 702 forms an extraordinarily stable ZrO2 passive film that resists boiling HCl up to 37% concentration and H2SO4 up to ~70% at boiling temperatures. Titanium Grade 7 uses 0.12–0.25% palladium as a cathodic depolarizer to extend CP titanium into dilute reducing acids (e.g., ~0.18 mm/yr in boiling 5% HCl), but experiences runaway active dissolution in boiling concentrated HCl (>15–20%).

The Oxidizing Impurity Trap (Fe³⁺ / Cu²⁺ / Cl₂): This is the #1 chemical plant selection mistake. Adding even 50–100 ppm of ferric chloride (FeCl₃), cupric ions (Cu²⁺), or free wet chlorine into HCl triggers severe localized pitting and stress-corrosion cracking on Zirconium 702. Conversely, those exact oxidizing ions stabilize Titanium Grade 7's TiO2 film and lower its corrosion rate.

Fabrication, Fluoride Exclusion & Lifecycle Cost: Both metals are destroyed by trace hydrofluoric acid (HF / free fluorides) and require high-purity argon shielding during GTAW welding. Titanium Grade 7 can be welded directly to economical Grade 2 structural shells and is typically 25–45% less expensive per cubic meter than Zirconium 702 (density 4.51 vs. 6.51 g/cm³).

Frequently Asked Questions: Zirconium 702 (UNS R60702) vs Titanium Grade 7 (Ti-0.15Pd)

Can Zirconium 702 be used in hydrochloric acid if ferric chloride (FeCl3) is present?
No. Even low ppm levels of oxidizing metal ions such as Fe³⁺ or Cu²⁺, or dissolved wet chlorine gas, can push Zirconium 702 past its pitting potential in HCl and cause rapid localized failure. In oxidizing chloride-acid mixtures, Titanium Grade 7 is the safer selection.
When should an engineer upgrade from Titanium Grade 7 to Zirconium 702?
Upgrade to Zirconium 702 when the process involves hot, uninhibited reducing hydrochloric acid above ~5–10% concentration near boiling, or hot sulfuric acid between 20% and 70% where Titanium Grade 7 exceeds its passive stability limit.
Can Titanium Grade 7 be welded directly to Grade 2 titanium?
Yes. Because Grade 7 is metallurgically identical to Grade 2 except for 0.12–0.25% palladium, it welds seamlessly to Grade 2 shells using ERTi-7 or ERTi-2 filler wire—whereas Zirconium 702 cannot be fusion-welded directly to titanium or steel due to brittle intermetallics.

Not sure which material is right for your project?

Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.

Related Comparisons

Ready to Start Your Project?

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Inquiry
WhatsApp