Titanium Square Bars
Also known as: Titanium Square Bar , Titanium Square Stock
Titanium square bars are square-section mill products supplied per GB/T 3621, hot-rolled or machined from round bar. The square section saves machining time for brackets, tool holders, frames and custom hardware compared with turning down round stock — available from stock and custom production in Baoji, China.
| Sizes | 6mm – 14mm square |
| Form | Square cross-section bars |
| Standards | GB/T 3621 |
| Available Grades | 2 grades |
Quick Factory Quote
⚡ 24h ResponseNeed pricing, availability, or custom cutting for Titanium Square Bars? Send your requirements or CAD/drawings directly to our engineering team.
Available Grades for Titanium Square Bars
Click a grade to view its chemical composition and mechanical properties inline.
Grade 1
Softest, most formable CP titanium with best ductility. Ideal for deep drawing, welding, and chemical linings.
Chemical Composition (wt%)
| Ti | Balance |
| Fe | 0.20 max |
| O | 0.18 max |
| C | 0.08 max |
| N | 0.03 max |
| H | 0.015 max |
Mechanical Properties
| Tensile Strength | 240 MPa – 345 MPa |
| Yield Strength | 170 MPa – 310 MPa |
| Elongation (min) | 24% |
| Hardness | 120 HB |
| Elastic Modulus | 103 GPa |
In stock 6/8/10/12/14mm
Titanium Square Bars Weight Calculator
Calculated Weight
Cost Estimate (FOB Baoji)
* Reference pricing only. Actual quote depends on specifications, tolerances, and certification requirements.
Grade 5 Properties
Request Quote for This Specification →
⚡ 24h Factory QuoteGet certified mill pricing & lead time for this exact specification.
Quality & Certification
Material Test Certificate
EN 10204 Type 3.1/3.2 MTC with every shipment. Full heat traceability.
Testing & Inspection
UT, PMI, tensile test, hardness test. Third-party inspection available.
Standards Compliance
Supplied to ASTM / ASME / AMS / GJB as specified. Approval scope confirmed per order.
Fast Delivery
Stock items: 3 days. Custom orders: 15–45 days. FOB Baoji / CIF worldwide.