Type something to search...

CP Titanium (Grade 1-4) vs Titanium Alloys (Grade 5, 9, 23) — Complete Comparison

Property CP Titanium (Grade 1-4) Titanium Alloys (Grade 5, 9, 23)
Strength Range (MPa) 240-680 620-1000 ★
Elongation (%) 15-24 ★ 10-15
Formability Excellent ★ Limited
Weldability Excellent ★ Requires expertise
Cost Lower ★ 40-100% higher
Heat Treatment Not heat treatable Heat treatable ★
Applications Chemical, marine, general Aerospace, medical, high-performance

Choose CP Titanium (Grade 1-4) When

  • ✓ Chemical processing tanks and piping
  • ✓ Marine heat exchangers
  • ✓ Deep drawing or forming needed
  • ✓ Budget-conscious projects

Choose Titanium Alloys (Grade 5, 9, 23) When

  • ✓ Aerospace structural parts
  • ✓ Medical implants
  • ✓ High strength-to-weight critical
  • ✓ Elevated temperature service

Not sure which material is right for your project?

Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.

Related Comparisons

Ready to Start Your Project?

Get factory-direct pricing on titanium products. No minimum order.

Get a Quote
Quick Inquiry
WhatsApp