TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) vs Grade 5 (Ti-6Al-4V) — Complete Comparison
Chinese TA15 (Ti-6.5Al-2Zr-1Mo-1V) and Russian GOST VT20 (ВТ20) are direct metallurgical equivalents—near-alpha titanium alloys engineered for 500°C continuous aerospace service (up to 3,000 hours)—extending operating temperature by 150°C beyond standard Ti-6Al-4V (Grade 5, capped at 300–350°C) while retaining superior fusion weldability.
| Property | TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) | Grade 5 (Ti-6Al-4V) |
|---|---|---|
| Alloy Class | Near-Alpha (Ti-6.5Al-2Zr-1Mo-1V) | Alpha-Beta (Ti-6Al-4V) |
| Regional Equivalents | TA15 (GB/T) = VT20 / ВТ20 (GOST) | Grade 5 / TC4 / VT6 (ВТ6) |
| Long-Term Max Service Temp (°C) | 500 (up to 3,000 hrs) ★ | 300–350 |
| Short-Term Flash Temp (°C) | Up to 800 (<5 min) ★ | ~400–450 |
| Room-Temp Tensile Strength (MPa) | 930–1,130 (annealed) ★ | 895–1,000 (annealed) |
| Fusion Weldability | Excellent (weld efficiency >90%) ★ | Good (requires strict PWHT) |
| High-Temp Creep Resistance | Superior (Zr + Mo stabilization) ★ | Moderate (<350°C) |
| Global Stock Availability | Made-to-order / specialized mills | Widely stocked globally ★ |
Choose TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) When
- ✓ Continuous operating temperatures between 350°C and 500°C
- ✓ Direct replacement for Russian GOST VT20 (ВТ20) forgings, plates, or bars
- ✓ Welded aerospace engine ducts, compressor casings, and thermal bulkheads
- ✓ High thermal creep resistance combined with >930 MPa room-temperature strength
Choose Grade 5 (Ti-6Al-4V) When
- ✓ Operating temperatures stay below 350°C
- ✓ Off-the-shelf global AMS 4928 / ASTM B348 stock and fast lead times are essential
- ✓ Standard airframe brackets, fasteners, and CNC structural parts
- ✓ Lowest alloy procurement cost with universal western qualification
Engineering Trade-Off Analysis: TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) vs. Grade 5 (Ti-6Al-4V)
Direct Equivalency Between TA15 and Russian VT20 (ВТ20): TA15 was developed under GB/T and GJB standards to match the chemistry and thermal stability of Soviet/Russian ВТ20 (Ti – 5.5–7.0% Al – 1.5–2.5% Zr – 0.5–2.0% Mo – 0.8–2.5% V). For global aerospace, turbine, and energy buyers replacing VSMPO-AVISMA VT20 forgings, bars, or plates, TA15 offers direct compositional and mechanical interchangeability when ordered to certified aerospace chemistry bounds.
Why TA15 / VT20 Outperforms Ti-6Al-4V Above 350°C: Standard Ti-6Al-4V is an alpha-beta alloy with 4% vanadium that softens and suffers unacceptable thermal creep above 350°C. TA15/VT20 uses high aluminum solid-solution strengthening combined with neutral zirconium (2%) and low beta-stabilizers (1% Mo + 1% V) to create a thermally stable near-alpha structure rated for 500°C continuous duty and 800°C short-duration (<5 min) flash exposure.
Weldability & Structural Forging Capability: Unlike many high-temperature alloys that crack during welding, TA15/VT20 exhibits weld joint strength coefficients above 0.90 of base metal, making it ideal for welded aero-engine casings, high-temperature ducts, and bulkheads. Mill delivery is available in annealed bars, plates, and ultrasonic-tested forgings.
Related Specifications, Grades & Mill Products
Frequently Asked Questions: TA15 / GOST VT20 (Ti-6.5Al-2Zr-1Mo-1V) vs Grade 5 (Ti-6Al-4V)
Is Chinese TA15 a direct drop-in equivalent for Russian GOST VT20 (ВТ20)?
What is the closest Western aerospace equivalent to TA15 / VT20?
Not sure which material is right for your project?
Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.
Related Comparisons
Grade Comparison
Grade 2 (CP Titanium) vs Grade 5 (Ti-6Al-4V)
Grade Comparison
Grade 5 (Ti-6Al-4V) vs Grade 23 (Ti-6Al-4V ELI)
Grade Comparison
CP Titanium (Grade 1-4) vs Titanium Alloys (Grade 5, 9, 23)
Grade Comparison
Titanium Grade 7 (Ti-0.15Pd) vs Titanium Grade 12 (Ti-0.3Mo-0.8Ni)
Grade Comparison
Zirconium 702 (UNS R60702) vs Zirconium 705 (UNS R60705)