Grade 2 (CP Titanium) vs Grade 5 (Ti-6Al-4V) — Complete Comparison

Property Grade 2 (CP Titanium) Grade 5 (Ti-6Al-4V)
Type Commercially Pure α+β Alloy
Density (g/cm³) 4.51 4.43 ★
Tensile Strength (MPa) 345-450 895-1000 ★
Yield Strength (MPa) 275-410 828-910 ★
Elongation (%) 20 ★ 10
Weldability Excellent ★ Good (requires care)
Cost Lower ★ Higher (~60% more)
Corrosion Resistance Excellent Excellent

Choose Grade 2 (CP Titanium) When

  • ✓ Chemical processing equipment
  • ✓ Heat exchangers and condensers
  • ✓ Weldability is critical
  • ✓ Cost-sensitive general corrosion applications

Choose Grade 5 (Ti-6Al-4V) When

  • ✓ Aerospace structural components
  • ✓ High strength-to-weight ratio needed
  • ✓ Medical implants
  • ✓ Elevated temperature applications

Not sure which material is right for your project?

Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.

Related Comparisons

Ready to Start Your Project?

Get factory-direct pricing on titanium products. No minimum order.

Get a Quote
Quick Inquiry
WhatsApp