Value Added Services
At Titanium Seller, we provide an extensive range of value-added services to enhance the quality, durability, and precision of our titanium products. Our services are designed to meet the demanding needs of various industries, ensuring that every solution is customized for performance and reliability.
1. Custom Titanium Fabrication Services
Titanium Seller offers custom titanium fabrication services tailored to your specific requirements. Our advanced fabrication capabilities include precision cutting, custom welding, and CNC machining to produce high-accuracy components that meet your exact project specifications.
Our Services Include:
- Precision titanium cutting
 - Custom titanium welding
 - CNC machining for intricate parts
 
2. Titanium Coatings & Surface Treatments
Our titanium coatings and surface treatments improve the functional and aesthetic qualities of your titanium products. We offer a wide range of options, including anodizing and sandblasting, to improve corrosion resistance and surface finish, ensuring that each product is ready for its specific use case.
Our Services Include:
- Anodizing for enhanced corrosion protection
 - Sandblasting to achieve smooth finishes
 - Custom coatings for added surface durability
 
3. Heat Treatment & Stress Relieving
Titanium Seller’s heat treatment services optimize the mechanical properties of titanium materials. Our controlled processes such as solution heat treatment and stress relieving improve the strength, fatigue resistance, and overall performance of your products, ensuring they meet the toughest industrial standards.
Our Services Include:
- Solution heat treatment for improved mechanical properties
 - Stress relieving to minimize internal stresses
 - Customized heat treatment tailored to your needs
 
4. Titanium Alloy Processing
We offer expert titanium alloy processing to meet the exact needs of your project. Whether it’s Ti-6Al-4V, Ti-5Al-2.5Sn, or other specialized alloys, our metallurgists ensure that the correct alloy composition is achieved for optimal performance in your specific applications.
Our Services Include:
- Titanium alloy selection and custom alloy formulation
 - Precision titanium alloy processing
 - Alloys for aerospace, medical, and industrial applications
 
5. Consultation & Design Services
Titanium Seller’s consultation and design services provide in-depth expertise to help you select the best titanium materials and engineering solutions for your needs. From initial consultation to final product delivery, our team offers support every step of the way to ensure efficient and effective project execution.
Our Services Include:
- Material selection and engineering advice
 - Design consultation for optimized solutions
 - Full engineering support from concept to production
 
6. Global Logistics & Supply Chain Management
Titanium Seller guarantees the efficient and secure delivery of titanium products worldwide. Our logistics and supply chain management team ensures that your orders are processed, shipped, and delivered on time, ensuring seamless operations for your business.
Our Services Include:
- Global shipping coordination to ensure timely delivery
 - Inventory management for effective order fulfillment
 - Real-time order tracking for complete transparency
 
Titanium Grades
At Titanium Seller, we work with a wide variety of titanium grades to meet the unique needs of various industries. Below is a breakdown of the most common titanium grades we supply, along with their typical applications:
| Grade | Composition | Properties | Applications | 
|---|---|---|---|
| Grade 1 | Pure titanium (99.5%) | Excellent corrosion resistance, very ductile | Chemical processing, marine environments | 
| Grade 2 | Pure titanium (99.2%) | Excellent corrosion resistance, good formability | Aerospace, industrial, medical applications | 
| Grade 3 | Pure titanium (99.0%) | Higher strength than Grade 2, moderate formability | Heavy-duty applications, heat exchangers | 
| Grade 5 (Ti-6Al-4V) | 90% Ti, 6% Al, 4% V | High strength, high temperature performance | Aerospace, biomedical implants, military | 
| Grade 7 | 90% Ti, 0.12% Pd | Superior corrosion resistance in reducing acids | Chemical processing, nuclear applications | 
| Grade 23 (Ti-6Al-4V ELI) | 90% Ti, 6% Al, 4% V, low interstitials | Low oxygen content, higher toughness and fatigue resistance | Aerospace, medical implants | 
| Grade 9 (Ti-3Al-2.5V) | 90% Ti, 3% Al, 2.5% V | Excellent fatigue strength, moderate corrosion resistance | Aerospace, high-performance applications | 