Commercially Pure (CP)
Grade 1
Commercially Pure Density 4.51 g/cm3
Tensile Strength 240–345 MPa
UNS R50250
chemical processing marine deep drawing
+1 more
View Details →
Grade 2
Commercially Pure Density 4.51 g/cm3
Tensile Strength 345–450 MPa
UNS R50400
chemical processing marine heat exchangers
+1 more
View Details →
Grade 4
Commercially Pure Density 4.51 g/cm3
Tensile Strength 550–680 MPa
UNS R50700
airframe fasteners cryogenic vessels
View Details →
Grade 7
CP + Pd Density 4.51 g/cm3
Tensile Strength 345–450 MPa
UNS R52400
chemical processing severe reducing acid environments
View Details →
Near-Alpha Alloys
Grade 9
Near-α Alloy Density 4.48 g/cm3
Tensile Strength 620–750 MPa
UNS R56320
aerospace hydraulic tubing bicycle frames offshore oil & gas
View Details →
Grade 12
Near-α Density 4.51 g/cm3
Tensile Strength 483–620 MPa
UNS R53400
heat exchangers chemical processing oil & gas sour service
+1 more
View Details →