Titanium Tolerance Calculator

Look up ASTM B265, B348, and B338 standard tolerances for titanium sheets, bars, and tubes by dimension.

Standard: ASTM B265

Available Ranges

0.4–0.6 mm±0.05
0.6–1.0 mm±0.08
1.0–2.0 mm±0.10
2.0–3.0 mm±0.15
3.0–5.0 mm±0.20
5.0–8.0 mm±0.30
8.0–12.0 mm±0.40
12.0–20.0 mm±0.60
20.0–40.0 mm±0.80
40.0–60.0 mm±1.20
60.0–100.0 mm±1.50
Enter a dimension to look up ASTM standard tolerances.