ASTM Standard

ASTM B265 Standard Specification for Titanium and Titanium Alloy Strip, Sheet, and Plate

Scope

Covers titanium and titanium alloy strip, sheet, and plate for general corrosion resisting and elevated temperature service.

Covered Product Forms

Sheet Strip Plate

Key Requirements

  • Chemical composition
  • Mechanical properties (tensile, yield, elongation)
  • Dimensions and permissible variations
  • Workmanship, finish, appearance

Test Methods

  • ASTM E8 (Tensile)
  • ASTM E120 (Chemical Analysis)
  • ASTM E29 (Rounding)

Related Specifications