Type something to search...
TA10 / Gr.12 Titanium-Molybdenum-Nickel Alloy Bars — Daily Production Update
  • By Jason/ On 08 Apr, 2026

TA10 / Gr.12 Titanium-Molybdenum-Nickel Alloy Bars — Daily Production Update

Today’s production spotlight: a fresh batch of TA10 / ASTM Gr.12 titanium-molybdenum-nickel alloy raw bars, stacked and marked on our workshop floor.

Material: TA10 (ASTM Gr.12 / Ti-0.3Mo-0.8Ni)

TA10 is a near-alpha titanium alloy with additions of molybdenum (0.2–0.4%) and nickel (0.6–0.9%). Compared to commercially pure titanium, Gr.12 offers significantly improved crevice corrosion resistance in hot brine, wet chlorine, and reducing acid environments — making it a go-to choice for:

  • Chemical processing — heat exchangers, reactor vessels, and piping
  • Oil & gas — sour-service downhole components
  • Marine desalination — evaporator tubes and plate heat exchangers
  • Power generation — condenser tubing in coastal plants

Today’s Batch

This run includes raw bars (unfinished billets) in two diameters:

DiameterGradeQuantity
Φ60 mmTA10 / Gr.12Multiple pieces
Φ75 mmTA10 / Gr.12Multiple pieces

Each bar is marked with its grade and diameter for full traceability through the production chain.

TA10 Gr.12 titanium alloy raw bars marked with grade and diameter

What Happens Next

These raw bars will be ultrasonically inspected, then machined or forged to customer specifications — turned bars, shafts, fastener blanks, or valve components. We can supply TA10 bar stock from Φ10 mm up to Φ300 mm, in both forged and rolled conditions.

Need Gr.12 titanium alloy bars or custom machined parts? Contact us for pricing and lead times.


Related Articles:

Need this material? Get a factory-direct quote.